Corrosion of Conductor Rolls in an Electrogalvanizing Line
Conductor rolls in continuous cold rolled steel strip horizontal acid electrogalvanizing lines after some period of service suffer a surface deterioration that alters its color, aspect and eventually its roughness what is more deleterious to its good performance. The surface degradation finally prod...
Autores principales: | Egli, Walter Alfredo, Seré, Pablo Ricardo, Bruno, S., Lazzarino, H. A. |
---|---|
Formato: | Articulo |
Lenguaje: | Inglés |
Publicado: |
2012
|
Materias: | |
Acceso en línea: | http://sedici.unlp.edu.ar/handle/10915/78422 |
Aporte de: |
Ejemplares similares
-
Corrosion of Conductor Rolls in the Electrogalvanizing Line at Sidercolor
por: Egli, Walter Alfredo, et al.
Publicado: (2012) -
Corrosion performance of electrogalvanizes steel treatment with Cr (III)-based products
por: Tomachuk, C., et al.
Publicado: (2011) -
Corrosion of conductor rolls in the electrogalvanizing line at Terniun
por: Egli, Walter Alfredo, et al.
Publicado: (2013) -
Susceptibility to SCC of FeCrNi alloys in 1M HCl solution
Publicado: (1991) -
Susceptibility to SCC of FeCrNi alloys in 1M HCl solution
por: Martinez, D.A., et al.