Kinetics of iron passivation and corrosion in molten alkali nitrates
The electrochemical behaviour of iron anodes in molten alkali nitrates has been investigated at temperatures ranging from ca 240–320°C. The E/I curves exhibit a potential region where the electrode passivates. Two different oxidized states of the passive iron surface exist. Within definite potential...
Guardado en:
Autores principales: | Arvia, Alejandro Jorge, Podestá, José J., Piatti, Roberto C. V. |
---|---|
Formato: | Articulo |
Lenguaje: | Inglés |
Publicado: |
1972
|
Materias: | |
Acceso en línea: | http://sedici.unlp.edu.ar/handle/10915/121835 |
Aporte de: |
Ejemplares similares
-
On the anodic passivity of iron in molten potassium bisulphate
por: Casino, R. G., et al.
Publicado: (1971) -
On the electrochemical behaviour of molten nitrites
por: Calandra, Alfredo J., et al.
Publicado: (1965) -
Changes in the kinetics of the oxygen evolution reaction induced by oxide films at platinum electrodes
por: Bolzán, Agustín Eduardo, et al.
Publicado: (1994) -
Kinetics and mechanism of the iron electrode in solutions of HCl in dimethylsulphoxide
por: Posadas, Dionisio, et al.
Publicado: (1971) -
Kinetics of the discharge of nitrite ions in the electrolysis of molten nitrites on graphite electrodes
por: Arvia, Alejandro Jorge, et al.
Publicado: (1967)