Load relaxation of cold-worked and stress-relieved Zircaloy-4 near 673 K
Load-relaxation data obtained for both cold-worked and stress-relieved Zircaloy-4 are presented. The stress-relaxation curves, plotted as the logarithm of the applied stress against time, are interpreted in terms of an anelastic plastic constitutive equation, whose plastic component involves jog-dra...
Guardado en:
Autores principales: | Povolo, F., Rubiolo, G.H. |
---|---|
Formato: | JOUR |
Materias: | |
Acceso en línea: | http://hdl.handle.net/20.500.12110/paper_01418610_v56_n2_p231_Povolo |
Aporte de: |
Ejemplares similares
-
Load relaxation of cold-worked and stress-relieved Zircaloy-4 near 673 K
Publicado: (1987) -
Model for the anelastic contribution to stress-relaxation at high temperatures
por: Povolo, F., et al. -
Model for the anelastic contribution to stress-relaxation at high temperatures
por: Povolo, Francisco
Publicado: (1987) -
Effects of dynamic strain ageing on the strain-rate sensitivity parameter of α-zirconium
por: Povolo, F., et al. -
Self-diffusion coefficient of α-zirconium
por: Marzocca, A.J., et al.