Liquid phase densification of Al-4.5wt.% Cu powder reinforced with 5wt.% Saffil short fibers during hot pressing
The Alumix 13 (wt.%) (Al-4.5 Cu 0.5 Mg 0.2 Si) powder with and without 5 wt.% Saffil short fibers specimens were hot pressed in the range 580-620. °C. The densification during pressure increase was fitted using the Konopicky model and an agreement with the associated linear plot P vs. ln(1/(1 - D) w...